Repair cracks by HM-120L crack injection adhesive

How to repair cracks can achieve better results? Shanghai Horse Construction summing up more than ten years of experience, we have to do these 12 points can better handle cracks

crack repair


We have to do 12 key points to improve the quality of crack repair.


1, The sealing quality directly affects the effect of the crack injection, so the closed surface cracks must be done well.


2. After the sealant has reached the curing time, then injection.


3, Accurately proportioning sealant.


4, The sealant must be stirred evenly, and there is no bubble mixing in the mixing.


5, The use of special glue injection equipment to injection sealant, and filling sealant with special irrigation equipment.


6, The cracks are dry.


7, The low pressure irrigation is used, and high pressure irrigation is not suitable.


8, Do not plug the vent when the glue is injected.


9. The order of glue injection is correct.


10, The curing temperature is above 0 centigrade.


11, The curing time depends on the temperature, the temperature is high, and the temperature is slow.


12, After the injection must be checked, the disqualification needs to be filled.




Các Sản Phẩm Được Gợi Ý của Horse Construction

Bạn có thể tìm thấy mọi thứ bạn cần ở đây. Hãy tin tưởng và thử nghiệm các sản phẩm này, bạn sẽ thấy sự khác biệt lớn sau đó.

Keo dán bịt vết nứt bê tông HM-9

Keo dán bịt vết nứt HM-9 là keo dán nhựa epoxy biến tính hai thành phần, thường được sử dụng với keo dán nứt đổ để bịt vết nứt và cố định vòi phun.

Thêm >

HM-120L Bê tông tiêm vết nứt Epoxy

Keo phun vết nứt bê tông Horse HM-120L là loại keo epoxy dùng để sửa chữa vết nứt bê tông bằng cách tiêm. Keo epoxy có tính thẩm thấu cao. Tiêm vết nứt ở áp suất thấp trong bê tông kết cấu.

Thêm >

Máy bơm keo

Máy bơm epoxy là dụng cụ bơm epoxy vào các vết nứt bê tông.

Thêm >

Back
Top
Close